getting CLOSURE // screw access pre-restorative photos are mandatory in case the limits are hard to discern when re-accessed in the future.
Zirconia should be adhesively bonded to using the #MarkusBlatz APC technique
A: Air Abrasion: 27 to 30 micron aluminum oxide at 30-40PSI or 2-3 bar.
P: Primer (MDP-containing primer)
C: Composite Resin
In this case a single shade of Voco Amaris O1 was used to layer and restore this screw access channel after screw coverage with PTFE tape.
#Voco #Amaris